作者:
Zixing,Wang [1]
;
Vidya,Kochat [1]
;
Prafull,Pandey [2]
;
Sanjay,Kashyap [2]
;
Soham,Chattopadhyay [3]
;
Atanu,Samanta [4]
;
Suman,Sarkar [4]
;
Praveena,Manimunda [2]
;
Xiang,Zhang [5]
;
Syed,Asif [1]
;
Abhisek K,Singh [5]
;
Kamanio,Chattopadhyay [4]
;
Chandra Sekhar,Tiwary [2]
;
Pulickel M,Ajayan [1]
作者单位:
Materials Science and Nanoengineering, Rice University, 6100 Main St, Houston, TX, 77005, USA.
[1]
Materials Engineering, Indian Institute of Science, Bangalore, 560012, India.
[2]
School of Engineering and Technology, BML Munjal University, 67th KM Stone NH-8, Gurgaon, 122413, India.
[3]
Materials Research Centre, Indian Institute of Science, Bangalore, 560012, India.
[4]
Hysitron Inc., Minneapolis, MN, 55344, USA.
[5]
DOI
10.1002/adma.201700364
PMID
28593718
发布时间
2020-09-30