Fatigue failure load of zirconia-reinforced lithium silicate glass ceramic cemented to a dentin analogue: Effect of etching time and hydrofluoric acid concentration.
第一作者:
Jaiane Bandoli,Monteiro
第一单位:
PhD Post-Graduate Program in Restorative Dentistry (Prosthodontics Units), Univ. Estadual Paulista (UNESP), Institute of Science and Technology at Sao Jose dos Campos, Sao Jose dos Campos, Sao Paulo State, Brazil. Electronic address: jaiane.monteiro@ict.unesp.br.
作者:
主题词
双酚A缩水甘油基异丁烯酸(Bisphenol A-Glycidyl Methacrylate);陶瓷制品(Ceramics);复合树脂类(Composite Resins);牙黏合(Dental Bonding);牙蚀(Dental Etching);牙瓷料(Dental Porcelain);牙应力分析(Dental Stress Analysis);氢氟酸(Hydrofluoric Acid);锂(Lithium);材料试验(Materials Testing);抗剪切强度(Shear Strength);硅酸盐类(Silicates);表面特性(Surface Properties);锆(Zirconium)
DOI
10.1016/j.jmbbm.2017.09.028
PMID
28988143
发布时间
2022-03-31
- 浏览6
相似文献
- 中文期刊
- 外文期刊
- 学位论文